Hi,
Please can you advise, a coating for 316 Stainless Steel (Instrument units) in Immersed / Buried Condition (High Water Table). For normal Temperature.
 
This is a standard of Norsok applicable to offshore Structure and equipment or piping, there is also a coating system for Stainless Steel.

This are some good article regarding painting of SS.


Paint coating stainless steels

Hope this help

S.

Metal Corrosion
 