shyamshins
Mechanical
Dear all forum members,
I am facing problem regarding seal which is used for sealing CO2 at -20deg. celcius.This is Single inside with cooled insert.
Product is CO2
Seal size is 1.875"
Suction Press.20.28kg/cm2
Disch.Press.29kg/cm2
Box press.20kg/cm2
Vap.press.20kg/cm2
Temp. -20 Deg.celcius
Sp.grv.1.07
Pump Rpm.2900. Make of pump is microfinish
When I install seal on pump it runs for 10 to 12 days and then it fails.This is used for unloading Liquid carbon dioxide CO2 from truck container.Flushing plan provided for this seal is API Plan 11 and it has lubricated insert which is lubricated by Ethylene glycol.
Problem was that carbon dioxide is entering pot which stores Ethylene glycol & pot press. rises. Lubricated insert has 2nos of orings which are of BUNA-N this happened 2 to 3 times I also checked for damage of O ring of insert but O ring is in good condition.
Request you to guide how I can solve this problem.
Red Flag
I am facing problem regarding seal which is used for sealing CO2 at -20deg. celcius.This is Single inside with cooled insert.
Product is CO2
Seal size is 1.875"
Suction Press.20.28kg/cm2
Disch.Press.29kg/cm2
Box press.20kg/cm2
Vap.press.20kg/cm2
Temp. -20 Deg.celcius
Sp.grv.1.07
Pump Rpm.2900. Make of pump is microfinish
When I install seal on pump it runs for 10 to 12 days and then it fails.This is used for unloading Liquid carbon dioxide CO2 from truck container.Flushing plan provided for this seal is API Plan 11 and it has lubricated insert which is lubricated by Ethylene glycol.
Problem was that carbon dioxide is entering pot which stores Ethylene glycol & pot press. rises. Lubricated insert has 2nos of orings which are of BUNA-N this happened 2 to 3 times I also checked for damage of O ring of insert but O ring is in good condition.
Request you to guide how I can solve this problem.