Hi guys,

does anyone know a way to do a wet environement CO2 corrosion test? Seems that Carbonic acid (formed into the water by the CO2) is not stable and that there is no way to qualify the compatibility of some material with wet environnement + CO2...

any clue?
 
Replies continue below

Recommended for you

Many thanks for your help, I will see with this ASTM doc what I can do..
 