kendalsimon
Industrial
We have some groups of small slots (2.3mm x 15mm) pitched 2.3mm apart on 1.2mm mild steel. When we cut, quite often a slug doesn't drop through the hole and sits up on the sheet so when it comes to the adjacent hole, the height sensor detects the slug instead of the sheet and focusses too high causing a really poor cut. Anybody had anything similar and found a solution? We are using all standard cutting conditions, 5" lens and Nitrogen as assist gas