Hi,

New to the forum here. Cheers to engineers.

I'm looking for a polymer that will go from clear to bright white.

This can be through any reasonable pathway that is safe for consumers, for example:

-Heating

-UV treatment

The polymer can be in a monomer state to start with or already polymerized

Let me know if you have any ideas, thanks,

Mike
 
How about blending in a small proportion of titanium dioxide powder? That's a pretty standard method.
 
Is there a way someone can do that at home?

I need something that an end user can treat at home to get the effect.

For example, something I was considering was a layer of monomer between two sheets of clear polymer... the monomer would then polymerize and turn bright white when the object was left in the sun.

Mike
 
Perhaps you should provide more details on the specific intent; there may be other alternatives.

TTFN
faq731-376
7ofakss
 
You need to talk to Chris DeArmit, check for posts by "Demon3", or look over in the polymer engr. forum.
 
Hello,

I developed and patented a material that does exactly that. It transitions reversibly when heated. More information can be found here:



Note however, the effect will be limited if the material thickness is too thin.

All the best,

Chris

Chris DeArmitt - PhD FRSC CChem
Plastic & Additives Webinars
Instant Downloads & Inexpensive
 
Does anyone know where the OP went? I answered his need but he doesn't see to have seen it.