Does anyone have the loss tangent and dielectric constant for Clear Anodize?

Thanks!
 
Replies continue below

Recommended for you

Electrical Properties. Aluminum oxide and its alloys can be used as electrical insulators. The high temperature stability of the coating permits operation up to 500C. Anodic coatings typically exhibit a voltage breakdown of 2,000-3,000 v/mil, a dielectric constant of 7.4-7.6 and resistivity from 1014 ohm cm to 200C. This resistivity is of the same order of magnitude as glass and porcelain.
 