Dear All,

which one is better for “Feed Stream Purification and portions of Vent Recovery Systems” - chemical or abrassive cleanning?
 
You'll probably need both methods, and more.


Mike Halloran
Pembroke Pines, FL, USA
 
no, I need to choose only one
 
It depends on the materials of construction, the length of the pipe networks, and the diameters of the pipes.
 
Selection of a cleaning technology also depends on what, exactly, you are trying to clean out of the pipe. The stuff I've seen in Vent Recovery systems required drifts, chisels and hammers just to recover enough lumen to begin thinking about other methods.

In any cleaning operation, you also have to worry about the volume and nature of the contaminated cleaning media you produce, what you're going to do with it, and how big a mountain of paperwork you'll need to originate, disseminate, get approved, process, archive, and eventually destroy.
... and what you're going to do with all that destroyed paperwok, and how big a mountain of paperwork you'll need to....

Selecting between chemical or abrasive cleaning, as the only permissible choices, and choosing just one, sounds like an academic exercise, conducted by a teacher who's never actually had to unclog a pipe In Real Life.




Mike Halloran
Pembroke Pines, FL, USA
 
Asys said:
no, I need to choose only one

This sounds like a multiple-choice test in some class at school.

If so, then Asys needs to go back to the books.

Sometimes its possible to do all the right things and still get bad results
 
I choose chemical. Boiling 37% Hydrochloric acid. That ought to do the trick!

Regards
StoneCold
 