Dear all,
which method is best and required for pitting corrosion between A923 method c and G48 method A.
regards.
 
A923 Test Method C is more defined for application to duplex and superduplex stainless steels. G48 testing in accordance with ISO 17781 is the current international standard for DSS/SDSS materials.

Steve Jones
Corrosion Management Consultant


All answers are personal opinions only and are in no way connected with any employer.
 