Oct 4, 2005 #1 harlequinir Chemical Joined Oct 23, 2003 Messages 8 Location US Can anyone recommend a cleaner (solvent or other) for removing a emulsified mineral oil (a CNC milling coolant)from a polished metal?
Can anyone recommend a cleaner (solvent or other) for removing a emulsified mineral oil (a CNC milling coolant)from a polished metal?
Oct 4, 2005 #2 NickE Materials Joined Jan 14, 2003 Messages 1,570 Location US Simple Green! Works great, is biodegradable, non-flammable... The only problem is that it leaves virtually nothing on the surface of the steel, so if not protected they'll rust. Upvote 0 Downvote
Simple Green! Works great, is biodegradable, non-flammable... The only problem is that it leaves virtually nothing on the surface of the steel, so if not protected they'll rust.
Oct 4, 2005 #3 EdStainless Materials Joined May 20, 2004 Messages 16,382 Location Waukesha WI USA TSP solution will work also. = = = = = = = = = = = = = = = = = = = = Corrosion, every where, all the time. Manage it or it will manage you. http://www.trent-tube.com/contact/Tech_Assist.cfm Upvote 0 Downvote
TSP solution will work also. = = = = = = = = = = = = = = = = = = = = Corrosion, every where, all the time. Manage it or it will manage you. http://www.trent-tube.com/contact/Tech_Assist.cfm
Oct 5, 2005 #4 SMF1964 Materials Joined Aug 5, 2003 Messages 306 Location US I've had good results with Dawn dishwashing detergent. Upvote 0 Downvote