hello - please excuse the way this question is asked so bear with me - we currently have a forging made from a694 f52 it is a very large round forging (60" in diameter)
while machining the part imperfections started showing up & the machining was stopped - after uting this part & others we may have to scrap the majority of these large parts -
is there any info as to what classifications for acceptance are allowed (depth, length, type of defect, etc.) that an inspector would use to say yes or no to the acceptance of a forging this large - the a694-f52 material spec refers to a961/a961m as the inspection criteria but does not give any classes of imperfection & under what circumstances or details this part is rejected or passed (this spec seems to refer to pipe & pipe falnges - not large forgings) - is a 1/16 deep by 1/8 long defect ok or not?? - if there is anything else i can add please let me know - thank you in advance
while machining the part imperfections started showing up & the machining was stopped - after uting this part & others we may have to scrap the majority of these large parts -
is there any info as to what classifications for acceptance are allowed (depth, length, type of defect, etc.) that an inspector would use to say yes or no to the acceptance of a forging this large - the a694-f52 material spec refers to a961/a961m as the inspection criteria but does not give any classes of imperfection & under what circumstances or details this part is rejected or passed (this spec seems to refer to pipe & pipe falnges - not large forgings) - is a 1/16 deep by 1/8 long defect ok or not?? - if there is anything else i can add please let me know - thank you in advance