Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations waross on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

class E grout

Status
Not open for further replies.

zennis

Structural
Oct 25, 2002
63
I am looking for specification on class E grout to be used for auger cast piles. Any information would be helpful.
 
Replies continue below

Recommended for you

I have used class D or Class D Modified grout:

D
Approximate Percent Fine to Total Aggregate
Gravel 35 Stone 39
Maximum Free Water by W/C Ratio (lb/lb)0.44
28-Day Compressive Strength(psi)4,000
Slump (inches) 3-5
Minimum Cement Factor (lb/yd3) 639
Air Content(%) 6 ± 2

D Mod
Approximate Percent Fine to Total Aggregate
Gravel 35 Stone 39
Maximum Free Water by W/C Ratio (lb/lb)0.42
28-Day Compressive Strength(psi)5,000
Slump (inches) 3-5
Minimum Cement Factor (lb/yd3) 733
Air Content(%) 6 ± 2
 