Hi,

I would like to know if a 3" Class 300 flange will bolt up with no problems to a 3" Class 600 flange? I work for a Process and Pipeline Company in Canada and we are going to be purging (with Nitrogen) a line for a client.

Due to such short notice all we have is a Class 300 flange and the tie in point we are using is a Class 600 (both raised face). There is no pressure on the line and will not have any other then the back pressure from us pumping Nitrogen.

Clay Culver
 
Replies continue below

Recommended for you

ASME B16.5 flanges, NPS 1/2 - 3 are identical flanges class 300, 400 and 600.
 