Hello All
When access from both sides are not possible, like welding clad pipe to clad pipe, generally the full joint is welded with the high alloy. (Clad pipe is CS + Incoloy 825). In this case ENi CR Mo-3 is used. This has been my experience.
Now a contractor is suggesting to use the following weld sequence(And is willing to support with a PQRT)
1) Weld the root with Er Ni Cr Mo-3
2) Second Run with E Ni Cr Mo-3
3) Next pass with carbon free Iron (Electrode/filler wire classification?)
4) Complete the joint with 7018-1
A)Is the above a common practice. Are there any flip side to the above suggestions?
B)What is the filler wire/electrode classification (AWS or SFA in Sec 2 c of ASME) for Iron electrode/Filler?
c)Is the above a stable weldment.
d)Somebody suggested welding Pure Nickel instead of Iron, is it true that Ni barrier instead of Iron will give a better weldment?
e)Can we permit above joints(Alloy + Iron + Cs) in a pressure vessel or Pressure plant piping or line pipe?
Thanks in adance
Moorthy
When access from both sides are not possible, like welding clad pipe to clad pipe, generally the full joint is welded with the high alloy. (Clad pipe is CS + Incoloy 825). In this case ENi CR Mo-3 is used. This has been my experience.
Now a contractor is suggesting to use the following weld sequence(And is willing to support with a PQRT)
1) Weld the root with Er Ni Cr Mo-3
2) Second Run with E Ni Cr Mo-3
3) Next pass with carbon free Iron (Electrode/filler wire classification?)
4) Complete the joint with 7018-1
A)Is the above a common practice. Are there any flip side to the above suggestions?
B)What is the filler wire/electrode classification (AWS or SFA in Sec 2 c of ASME) for Iron electrode/Filler?
c)Is the above a stable weldment.
d)Somebody suggested welding Pure Nickel instead of Iron, is it true that Ni barrier instead of Iron will give a better weldment?
e)Can we permit above joints(Alloy + Iron + Cs) in a pressure vessel or Pressure plant piping or line pipe?
Thanks in adance