Vindicit
Mechanical
- May 24, 2016
- 38
So Im trying to understand circularity and I thought I had a grasp on it until I see how some of my parts are measuring up in this metrology software. The picture shows a ring with a certain diameter and the only tolerance on there is the .035 circularity tolerance. The reading shows up at .016. The software is setup to show yellow lines when the tolerance is 75% or over. So the reading of .016 isnt even half of the tolerance. The reading at the point of yellow is about .010 off nominal. Does anyone understand how this could be showing up as yellow?