Hello,

I was wondering if anyone here has ever heard of a company that would manufacture chrome-magnesite crucibles (for lab tests). A colleague would like to simulate a pyrometallurgical process in the lab and wants to use this for the crucible material.

Thanks very much

D
 
At one time it was no problem getting CM crucibles from any foundry or refractory supply store until the demise of all the refractory companies. The last CM crucibles I saw came from A P Green prior to their dismantlement.

Here is whats left of several refractory companies operating under to two umbrella companies. I would give them a call and if they don't have CM crucibles they probably know where you might find them.



As you are looking a small number and smaller size you might want to give Legend a call. Or do a search under "assay crucibles +fire" as there is one hell of a lot of activity in this area at the present time.


Small CM crucibles are also used in thermite welding.
 
Thanks very much unclesyd. I will look into this some more.

You really are the master of answers in this site!