Hello all,

I have evidence of chromium depletion in 304H butt welds from metallurgical analysis. The depletion appears to be the result of high heat input / slow cooling.

I want to develop a presentation for our trades people and wondering if there are any "canned" materials out there similar to this.
 
Thank you gentlemen, great links.
 