Choice Between Higher Steel Grade and Higher Wall Thickness 3

Status
Not open for further replies.

Chembloke99

Chemical
Joined
May 6, 2009
Messages
23
Location
AU
Hello,

I would like to know from both technical and commercial point of view if I have to make a choice for a subsea pipeline between Higher Steel Grade and Higher Wall Thickness, which one I should go for?

For e.g. , for a 6" pipeline should I go for API 5L X- 52 Wall Thickness - 12.7 mm or

API 5L X 65 and Wall Thickness - 10.97 mm.

Many Thanks.





 
They both work and he has to decide which one is the cheaper solution. Since he hasn't built the line yet, nothing's changed.

**********************
"The problem isn't working out the equation,
its finding the answer to the real question." BigInch
 