Does anybody know where I can find information about ranges of Chloride in Concrete? I am looking for nominal ranges to compare test results to. Thanks
 
Check with your state Department of Transportation for relevant water soluble chloride limits in your area. Generally, chlorides are limited to no more than about 0.4 percent by weight of cement. Another limit is about 1 to 2 lbs per cubic yard.
 