grayseal
Materials
- Jun 29, 2001
- 78
I am looking for a standard test (ASTM preferred) for the detection of the chloride ion. My application involves the corrosion of 300 series stainless steel autoclaves. I have some information about utilizing silver nitrate.
grayseal