I am being asked to investigate yellow Alodine versus Chemical Film RoHS compliant. My understanding is that yellow Alodine contains hexavalent chromium, and is therefore, not RoHS compliant.
I just asked our metal finisher about dyeing the RoHS compliant finish, and he tells me that it is not yet possible.
Is anyone aware of a conductive, coloured RoHS compliant chemical film?
What sort of a future does hexavalent chromium chemical film have? Any?
--