Code : ASME Section VIII Div 1
Plate: A516 Gr 70 + SS 316L
======================================
Welds that are exposed to the corrosive service fluid need to maintain the corrosion resitance properties as much as possible and it is prefered that the chemical composition of the back cladding welds meet as closely as possible the clad material composition.
But how "closely" should it be? Will the ferrite count of 3-8% be adequate?
Please advise.
Plate: A516 Gr 70 + SS 316L
======================================
Welds that are exposed to the corrosive service fluid need to maintain the corrosion resitance properties as much as possible and it is prefered that the chemical composition of the back cladding welds meet as closely as possible the clad material composition.
But how "closely" should it be? Will the ferrite count of 3-8% be adequate?