How can I calculate Characteristic element length and Fracture energy for Damage evolution in ductile damage module in ABAQUS?
Suppose that:
1-The model has S4R shell element
2- The finest element shape is like the picture
3- Type of mesh is Orphan mesh
4- Total Fracture area below the Stress-Strain Curve is 60
mesh_shape_g0gfl8.jpg
 
Replies continue below

Recommended for you

Check the documentation chapter "Damage evolution and element removal for ductile metals", it describes it all in detail. You don’t have to define characteristic length, just the fracture energy.
 
FEA way You are right but I don't know how to calculate fracture energy. It depends on L and Total fracture area.
L_nn4bfs.jpg
 
To define fracture energy you can use the area under stress-strain curve that you've mentioned before. Hilleborg's model is really common so you should be able to find some additional resources besides the Abaqus documentation.
 