I am working in the QA Industry. I have been advised that a caompnay has brought over another company and has retained the wedlers and the qualified procedures. The new company is asking us to re-issue the certificates under the ASME code requirements. Is this allowable and what is the burden of proof we need to see

Regards

bigian
 
See Interpretation IX-95-40
File BC93-431 and BC95-222
I have reproduced the same below for your reference
Background: Company A was a subsidary of Company B. Company B sold Company A to Company C, and Company A became a division of Company C.
Question: May Co A continue to use WPSs and PQRs previously developed by Co B?
Reply: It is the intent of the Code that when a manufacturer or contractor or a part of manufacturer or contractor , is acquired by a new owner(s), the PQRs and WPSs may be used by the new owner without requalification, provided all the following are met:
a) the new owner(s) takes responsibilty for the WPSs and PQRs;
b) the WPSs reflect the name of the new owner(s); and
c) the Quality Control System/ Quality Assurance Program reflects the source of the PQRs as being from the former manufacturer or contractor.


Does this answer your question Thanks and regards
Sayee Prasad R
Ph: 0097143968906
Mob: 00971507682668
End of all knowledge is the attainment of immortality!
 
See ASME SecIX QW-201.1 and QW-300.2d Discuss with your AIA.
 
DeanC,
The references mentioned above ASME SecIX QW-201.1 and QW-300.2d do allow the WPS and welders to be used with change in ownership. Does it still require to be discussed with AI? Thanks and regards
Sayee Prasad R
Ph: 0097143968906
Mob: 00971507682668
End of all knowledge is the attainment of immortality!
 
You need AIA acceptanc of your QC system and program changes. If you wish to avoid problems later always consult your AI.
 