If your tube wall is also 1m thick, then the change in wall thickness for a given change in bulk temperature should be similar to the change in length if the tube is made from a typical metal. If the tube material is unconstrained and heated uniformly, then it should experience a consistent linear thermal expansion rate in all directions.