dear all,

I have doubt in thermal expansion of tube. if I heat a tube of 1m length,
why the increase in length is higher than the increase in thickness?
what will be the ratio of length to thicknes change in tube?
 
If your tube wall is also 1m thick, then the change in wall thickness for a given change in bulk temperature should be similar to the change in length if the tube is made from a typical metal. If the tube material is unconstrained and heated uniformly, then it should experience a consistent linear thermal expansion rate in all directions.
 
what will be the ratio of length to thicknes change in tube?
The same as the ratio of length to thickness in original tube