confused859
Mechanical
This may be a bit bizarre but I was given this problem to solve. I need to anchor a 3/4" chain (grade 100 - 113 kips minimum breaking force) to a concrete deadman (6' long, 3' wide, 6' deep). The client wants to wrap the chain around an embedded steel bar (3" in diameter) near the bottom of the deadman (6-12" from the bottom surface).
I realize the deadman is too small to develop the full strength of the chain, but I would like to consider a hypothetical load of 100 kips.
Any advice on calculating the holding force of this type anchor? Also any advice on rebar size and spacing would be great.
I realize the deadman is too small to develop the full strength of the chain, but I would like to consider a hypothetical load of 100 kips.
Any advice on calculating the holding force of this type anchor? Also any advice on rebar size and spacing would be great.