I am having random issues with scratch marks on the pieces coming out of my centerless grinders. In particular 3 distinct parts are all having this issue across sealing surfaces. I feel like the issue may be pieces of the grinding wheel or some of the metal removed at the previous process is sticking to the parts and causing issue at the next grind process. All three machining centers share a coolant reservoir which is filtered. My question, is it possible the coolant fluid is too viscous and allowing those particles to stick to the parts and transfer to the next grinder where they are scoring the parts? any other recommendations or things I could look into to try and stop these scratches?