Hi,
I have questions regarding CBR test for subgrade /subbase/road base material that include compaction stage(sampel prep) - soaking stage - peneteration stage.
1. Stated in BS that the during preparation of sample/compaction test, solid base plate shall be used, then change to perforated base plate during soaking stage and then change to solid base plate for the penetration stage. If for testing testing subgrade, sub base & roadbase, the perforated base plate to be used from the preparation of test until penetration test (means no solid base plate is used) Will this affect any result?
2. is the weight of the surcharge disc used during soaking stage will affect the whole process? Because i know the surcharge simulate the effect of the thickness of road pavement overlying the layer being tested. or any weight will be sufficient?
3. The dry density for the material calculated using bulk density of the soaked material or bulk density after compaction stage?
Thank you and please anyone can give opinion.
I have questions regarding CBR test for subgrade /subbase/road base material that include compaction stage(sampel prep) - soaking stage - peneteration stage.
1. Stated in BS that the during preparation of sample/compaction test, solid base plate shall be used, then change to perforated base plate during soaking stage and then change to solid base plate for the penetration stage. If for testing testing subgrade, sub base & roadbase, the perforated base plate to be used from the preparation of test until penetration test (means no solid base plate is used) Will this affect any result?
2. is the weight of the surcharge disc used during soaking stage will affect the whole process? Because i know the surcharge simulate the effect of the thickness of road pavement overlying the layer being tested. or any weight will be sufficient?
3. The dry density for the material calculated using bulk density of the soaked material or bulk density after compaction stage?
Thank you and please anyone can give opinion.