I am using Hardwear 400F in a caustic (pH=14) and heavy abrasion application, in the chemical industry (dissolving of sodium silicate). The equipment handles a caustic solution of sodium silicate and water. It is lined with the Hardwear and runs at temps btwn. 250 and 400 deg. F.
Hardwear 400F is hard to find. Any suggestions for an equivalent material?