I found the cracks shown in these photos in a concrete pathway. The cracks seem like a "grid-pattern", and also they seem to be perpendicular to sawn joints.
Just wondering what can cause this pattern and why the slab would crack perpendicular to the sawn joint although the joints are places to make the pathway square in shape?