Eng-Tips is the largest forum for Engineering Professionals on the Internet.

Members share and learn making Eng-Tips Forums the best source of engineering information on the Internet!

  • Congratulations JStephen on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Cathodic protection UST

Status
Not open for further replies.

cjfam

Civil/Environmental
Joined
Jul 26, 2007
Messages
1
Location
US
I have a railcar that we will be burying and using as part of a water cooling system. It is stainless steel and is about 18,000 gallons. Does anyone have tips regarding sizes and materials for cathodic protection for this application. I do not know the soil conductivity yet.

Thanks
 
Stainless steel doesn't require protection in most soils. Also, cathodic current could undo the normal passive oxide film on the SS. Can we presume 304 SS?

Analyze the soil for salinity (actually, Cl- & F-), pH and anything like sulfide that might feed nasty microbes.
 
The first tip is to coat the item with a carefully selected and qualified coating system. A thermal spray coating may alleviate any need for CP arising from your soil corrosivity assessments.

Steve Jones
Materials & Corrosion Engineer
 
Status