Apr 25, 2023 #1 sarawana Mechanical Joined Oct 10, 2020 Messages 23 Location IN dear, What is the principle of cathodic protection ion pressue vessel?, where it can applicable? And what is the purpose of anode & cathodic in pressure vessel.
dear, What is the principle of cathodic protection ion pressue vessel?, where it can applicable? And what is the purpose of anode & cathodic in pressure vessel.
Apr 27, 2023 #2 Dhurjati Sen Materials Joined Dec 14, 2017 Messages 1,005 Location IN Putting zinc anodes in the channel box of carbon steel coolers is an example. Google to find out more about cathodic protection. DHURJATI SEN Kolkata, India Upvote 0 Downvote
Putting zinc anodes in the channel box of carbon steel coolers is an example. Google to find out more about cathodic protection. DHURJATI SEN Kolkata, India