I often investment cast bronze, but customer demand is asking for 17/4PH, strong when heat treated, and holds a sharp edge well. Not having any luck finding info on casting of this metal. Any help appreciated.

Ken
 
Fighting to withold wisea** comments

I "Googled" "17-4ph casting" and came up with this web site on the top of the list:


There were other links on the google return, you should check it out.

Still fighting smarta** comments....
Must select "Submit Post" now..
 
monkeydog,
i have added the link into my bookmarks, along with all the other links which i classify as "worthless" hehehhe

I am after actual casting info.
what procedures need to be followed, eg, actual pouring temps, what fluxes or covers are needed, precautions to avoid gas pickup or loss of alloys, etc.


Ken
 
You can contact SFSA for technical help. Also AFS has a wing on Investment casting. This is advised as you are seeking complete knowhow to invest cast 17/4PH castings.
 
Thankyou arumrao!

 
I've had parts investment cast in 17/4PH. They were done somewhere in South Africa, but I've lost the contact info.
 
17-4 is a common casting material. The alloy supplier can give the standard practices.
 