Hello,
We are procuring Grey cast Iron casting (GG25) from one of the supplier.
Supplier has checked in 10 spots and certified the casting to 185-200BHN using Poldi hammer. He also has certified UTS value as 305MPa.
Supplier then shipped the casting to Europe.
When European plant checked the casting in the same spots using Ernst method, we are getting 150-160 BHN. (Spec. is 170-220BHN). Re-check was conducted with two operators to remove the operator variability. Plant also reports that they used Portable Briness hardness tester to verify in one spot (where feasible) and the hardness is same.
Now, I want to understand the reason for this difference in hardness value. Any inputs on where I have to look, is appreciated.
We are procuring Grey cast Iron casting (GG25) from one of the supplier.
Supplier has checked in 10 spots and certified the casting to 185-200BHN using Poldi hammer. He also has certified UTS value as 305MPa.
Supplier then shipped the casting to Europe.
When European plant checked the casting in the same spots using Ernst method, we are getting 150-160 BHN. (Spec. is 170-220BHN). Re-check was conducted with two operators to remove the operator variability. Plant also reports that they used Portable Briness hardness tester to verify in one spot (where feasible) and the hardness is same.
Now, I want to understand the reason for this difference in hardness value. Any inputs on where I have to look, is appreciated.