I have questions regarding casting definition.
I will try and describe the issue and the questions without a picture or drawing. I think this will be ok.
I have a complex investment cast part/shape with primary/secondary/tertiary datums. Two lugs defined by a basic radius of .XXX establish the primary 'datum axis' E-F through the two lugs. A third lug defined by a basic radius of .XXX establishes the secondary datum G. A .250 diameter spot defined by basic X/Y dimension from one of the lug radii on a surface of one of the lugs establishes the tertiary datum H and constrains translation.
The engineering drawing consists of iso views which show the part and the datum structure with a note that states " Geometry defined by solid model XXXXXX-D-1 Rev X. Cast cores shall lie within a profile tolerance of .XXX relative to datums E-F, G and H. Other cast features shall lie within a profile of .060 relative to datums E-F, G and H.
My questions:
Can the cast datum lugs vary in size by the profile tolerance of .060?
The answer leads to this summary.
If I mount each part (I pick 20 for a sample) in a fixture which adequately locates on the lugs E, F, G and the point H (lugs E-F establish a datum axis E-F). I would expect any feature on the surface of all 20 parts to lie with profile of .060 relative to datum structure? This includes variation in datum size.
I will try and describe the issue and the questions without a picture or drawing. I think this will be ok.
I have a complex investment cast part/shape with primary/secondary/tertiary datums. Two lugs defined by a basic radius of .XXX establish the primary 'datum axis' E-F through the two lugs. A third lug defined by a basic radius of .XXX establishes the secondary datum G. A .250 diameter spot defined by basic X/Y dimension from one of the lug radii on a surface of one of the lugs establishes the tertiary datum H and constrains translation.
The engineering drawing consists of iso views which show the part and the datum structure with a note that states " Geometry defined by solid model XXXXXX-D-1 Rev X. Cast cores shall lie within a profile tolerance of .XXX relative to datums E-F, G and H. Other cast features shall lie within a profile of .060 relative to datums E-F, G and H.
My questions:
Can the cast datum lugs vary in size by the profile tolerance of .060?
The answer leads to this summary.
If I mount each part (I pick 20 for a sample) in a fixture which adequately locates on the lugs E, F, G and the point H (lugs E-F establish a datum axis E-F). I would expect any feature on the surface of all 20 parts to lie with profile of .060 relative to datum structure? This includes variation in datum size.