We are looking to change our existing alloys for investment casting from 431 stainless steel to 4130 or 17-4 ph. We then saltbath nitride the parts. We want to reach a Rc of around 30-34 Rc to prevent the parts to become too brittle but keep a good wear characteristic.
Which alloy would be the best choice and why?