I have a Twin Otter Nose Wheel is cast magnesium, yet I don't have any further info on it regarding the manufacturing spec. MIL-HNDBK-5 lists seven different specs for cast magnesium as follows,
AM100A
AZ91C
AZ91E
AZ92A
EZ33A
QE22A
ZE41A
Does anybody have any suggestions for identifying the type of casting I have here? I’m not getting any support from the OEM…
Thanks,
Phil
AM100A
AZ91C
AZ91E
AZ92A
EZ33A
QE22A
ZE41A
Does anybody have any suggestions for identifying the type of casting I have here? I’m not getting any support from the OEM…
Thanks,
Phil