I have a drawing for a spindle clamp that calls out the following material: G00 UNI 5007-69. Do you know where I can find some technical information on this material? Is there an equivalent grade in the US market?

I have not be able to find any information relating to this material.

Thanks.
 
Replies continue below

Recommended for you

UNI 5007 Grey iron for castings. Qualities, requirements and tests covers gray iron castings (flake graphite). A similar standard in the US is ASTM A 48 Standard Specification for Gray Iron Castings.

I don't think G00 is an accurate designation. Possibly a misprint?

Regards,

Cory