Thanks mrfailure!
However, I meant to ask why ASTM A278 material doesn't list a yield strength. My thought was maybe it doesn't yield before breaking. Hence, only a UTS is listed.
Like you said, ASTM A47 is malleable with a yield of 220 MPa and UTS of 340 MPa. How can I compare an electric motor frame mounted with four bolted feet made of these two different cast materials (the 220 MPa yield of A47 with the 200 MPa UTS of A278)?
Thanks again
mauner