I am considering making support for large gear during carburize cycle. Fixture is to be re-usable also. We normally used low carbon steel with decent success.
My question is whether there is any benefit to using cast iron instead, either by cost savings or durability.
Cylce will be 1700 F for approx 10 hours.
Support Ring will be 18.5" OD, 15" ID, 1.5" thick
Part weighs about 88 lbs.
Thanks
My question is whether there is any benefit to using cast iron instead, either by cost savings or durability.
Cylce will be 1700 F for approx 10 hours.
Support Ring will be 18.5" OD, 15" ID, 1.5" thick
Part weighs about 88 lbs.
Thanks