Hello all,

I hope it is the right forum for it.
I would like to know where can I find the mechanical properties of A356-T6 aluminum casting as function of temeprature.

I want to know what is the yield strength and the elastic modulus at 125°C.

Thank you very much
 
Sand cast or permanent mold cast?
 
ASM Handbook