What cast aluminum alloy and heat treatment would you recommend for a cast aluminum blower. The material thickness varies from about 1/2" to 3/16". The diameter range is 18" to 32" maximum. The operating speed is 3550 rpm. The blower impellers will operate at ambient temperatures in a non-corrosive environment. Some suppliers have suggested 319, 356-T6, A356-T6, A357-T61. I would appreciate your comments and/or recommendations and your reasoning for the selection.