Is there a wrought grade equivalent to the cast C86500 Manganese Bronze?
 
Replies continue below

Recommended for you

No, I did not find an equivalent wrought material for the cast version C86500. Depending on the application, you will need to substitute a completely different wrought copper alloy that can have similar corrosion resistance and mechanical properties.
 