HI ALL

CAN ANYONE TELL ME OF A STANDARD FOR EVALUATING RESULTS OF CASS TESTS.
THE COMPONENT CURRENTLY UNDER TEST IS; FeC BASE METAL, BRONZE / CHROME PLATING, WITH A PLATING DEPTH OF 75 - 100 MICRONS.
GRADES OF 10 AFTER 1000HRS ARE ACHIEVED USING NSS TESTING, WHICH HAS LED ME USE A MORE AGRESSIVE FORM OF TESTING.
IF THERE IS NOT A STANDARD CAN ANYONE POINT ME IN THE DIRECTION OF INFORMATION?

BEST REGARDS

STEVE





 
Replies continue below

Recommended for you

We have an internal standard consisting of assessing the number of rust particles per unit area. I suggest for more information try posting this queery on the page.
 