Hi
Im envolved in a situation where the contractor has done partial penetration fillet welds on MS truss joints with the electrode used is E7018 without any baking.
Having the right to order to redo the weld.
And adopting AWS D1.1.
Would you recommend that? Would there be any possibility for the steel members losing its strength on the grinded welds that has to be redone? We are looking at 40 joints.
Can we avoid redo the weld by conducting package of NDT tests?
The problem here the weld is not full penetration puting limitation in this choice.
My highest priority is not to tolarate for the quality and service life of the structure. Time comes secondary here.
Highly appreciate your inputs
Im envolved in a situation where the contractor has done partial penetration fillet welds on MS truss joints with the electrode used is E7018 without any baking.
Having the right to order to redo the weld.
And adopting AWS D1.1.
Would you recommend that? Would there be any possibility for the steel members losing its strength on the grinded welds that has to be redone? We are looking at 40 joints.
Can we avoid redo the weld by conducting package of NDT tests?
The problem here the weld is not full penetration puting limitation in this choice.
My highest priority is not to tolarate for the quality and service life of the structure. Time comes secondary here.
Highly appreciate your inputs