According to Code Case 2235-6, (C) state that "The qualification block(s)shall be prepared by welding or HIP......,oriented to simulate flaws parallel to the production weld's fusion line... "

Question 1).The qualification block(s) shall be contain with a welded joint?

Question 2). If the qualification block(s) contain a welded, done welded joint configuration shall be same with production vessel...?

Regards

 
Replies continue below

Recommended for you

Question 1).The qualification block(s) shall be contain with a welded joint?

You need to duplicate a cast structure. This can be done by HIPing or a welded coupon (this would contain a weld joint).


Question 2). If the qualification block(s) contain a welded, done welded joint configuration shall be same with production vessel..

It can be.
 