Speicifically I am looking for yield strength for A36 or A516-60 at 1200°F. Required for some 'thermal straightening' calcs ... thanks in advance.
 
Replies continue below

Recommended for you

Reduction factor at 1200 deg F is around 0.3,

YS *.3

Source - Mechanical Properties of Structural Steel at Elevated Temperatures and After Cooling Down

Jyri OUTINEN and Pentti MÄKELÄINEN
Laboratory of Steel Structures,
Department of Civil and Environmental Engineering,
Helsinki University of Technology
P.O. Box 2100, FIN-02015 HUT, Finland
 
Thanks metengr - I was able to google a full copy of the paper.
 