Hello,

I am reviewing a proposal to replace a 16" diameter nozzle with a 20" nozzle on a distillation column. The column has a carbon steel outer shell 39/64" thick, 316 SS clad liner 5/64" thick and then 904L strip lining 10 GA thickness. They are proposing to provide a carbon steel nozzle cladded with AL6XN, since it is more readily available then 904L. Are there any pro's or con's to this compared to a solid AL6XN nozzle? Is it preferable to avoid dissimilar material welding between the carbon steel shell and an AL6XN nozzle? Any other factors to consider? I am having difficulty locating material of construction information for the existing 16" nozzle.

Thank you,

Dee
 
Will the new one be made from clad plate? Like explosively bonded?
If the column is lined then what is the issue?
I would rather see steel welded to steel with the alloy liner than trying to weld solid AL-6XN to steel.

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, Plymouth Tube
 
Excellent. Got the message loud and clear. Much appreciated to the two of you.