WE HAVE AN REQUIREMENT FOR CARBON MOLYBDENUM STEEL, AS PER ASTM A352 CARBON MOLYBDENUM STEEL IS LC1 MATERIAL(CAST GRADE), IF WE USE FORGED FORM OF CARBON MOLYBDENUM STEEL THEN WHICH WILL BE THE CORRECT MATERIAL, AS I CHECKED THERE IS NO EQUIVALENT FORGED GRADE FOR CARBON MOLYBDENUM STEEL.
 
Replies continue below

Recommended for you

Dear N AHMAD,

Don't go by the composition alone. Compare the tensile and impact properties too. You should find a near match in ASTM A 350.

Regards.

DHURJATI SEN
Kolkata, India

 