Hello,
I have to do a finite element analysis with ANSYS of a commercial carbon fibre tube. If have no information about the different layers of the tube.
All material properties I have are the following:
I assume that the material data I have to define in ansys is:
EX=2.5*10^6
EY=8.7*10^6
GXY=0.8*10^6
PRXY=0.43
Am I right?
But with these propertys I will only be able to do a 2-D analysis with plane elements. Will it provide me satisfactory results?
What data may I use, if I want to do an analysis with shell elements or volume elements?
I would be deeply grateful if you could give me any hints.
I have to do a finite element analysis with ANSYS of a commercial carbon fibre tube. If have no information about the different layers of the tube.
All material properties I have are the following:

I assume that the material data I have to define in ansys is:
EX=2.5*10^6
EY=8.7*10^6
GXY=0.8*10^6
PRXY=0.43
Am I right?
But with these propertys I will only be able to do a 2-D analysis with plane elements. Will it provide me satisfactory results?
What data may I use, if I want to do an analysis with shell elements or volume elements?
I would be deeply grateful if you could give me any hints.